Fiber Sizing Should Be Considered In Sizing Auxiliaries.
When sizing yarn, it is difficult to achieve the desired sizing effect when using one or several main sizing agents. It is necessary to use various auxiliaries as auxiliaries to improve the slurry performance.
The use of auxiliaries is small, but there are many varieties and different properties. Only by fully understanding the characteristics of various auxiliaries can we correctly select the types of auxiliaries and improve the sizing quality according to the types of fibers, yarn structure, fabric specifications, weaving conditions and characteristics of the main slurry itself.
The selection and use of auxiliaries are closely related to sizing effect, and their uses are manifold.
When a certain type of auxiliaries are used to get better results in a certain area, they often produce unfavorable results on the other hand.
In order to make the film soft and round, grease is often used, but the oil will weaken the strength of the serous membrane and the adhesive force of the pulp to the fiber, thereby reducing the abrasion resistance and the enhancement rate of the sizing.
Therefore, it is very important to choose the type and dosage of the auxiliaries correctly.
The additives should first have the characteristics of mixing any other slurry into a uniform slurry at any temperature below 100 degrees Celsius. It does not volatilize or decompose at high temperature, and there should be no chemical reaction that deteriorates the quality of slurry between all kinds of slurry. It should not damage the properties of the fiber, and it is easy to desalter the machine without corrosion.
Secondly, the use of auxiliaries can not affect finishing after printing and dyeing, and does not damage the fabric style, and does not affect the fabric color.
More importantly, the price is reasonable, the source is adequate, and the use is convenient.
Under normal conditions, the amount and type of auxiliaries should be used as little as possible when weaving conditions are met.
Commonly used auxiliaries are: surfactants, oils, waxes, preservatives, etc.
When sizing, it is desirable not only to have a more complete film on the surface of the yarn, but also to have a certain amount of slurry immersed in the yarn. Therefore, a proper amount of surfactant should be used.
The concentration of surfactants in the slurry should be slightly higher than the critical micelle concentration, and the concentration is too high. It will not only cause no effect, but also cause the aggregation of molecules, which will bring adverse effects on the technological properties of the slurry.
Anionic and non release surfactants are generally used as auxiliaries for sizing agents.
The surfactants are divided into wetting agents, penetrating agents, dispersing agents, antistatic agents in warp sizing.
Emulsifier
Defoamers and foaming agents.
Commonly used soaking agents are Turkey red oil, sallow oil, brown or yellow oily liquid, and soaking agent for textile, and O, 5881D, soap and so on.
There should not be too much impregnating agent, otherwise the slurry will blister easily.
When sizing agent is added with emulsifier in the slurry, the emulsifier molecules adsorb on the two phase interface and form an adsorption layer.
It is worth noting that since NPEO and NP are all non degradable substances, NPEO, OPEO, NP and OP in APEO have been included in the detection range since January 2012 and can not be used.
Enterprises should switch to environmentally-friendly emulsifiers such as isomeric 13 alcohol series.
In weaving process, yarn tends to form electrostatic accumulation, and adjacent warps are easily entangled, resulting in unclear weaving, flying flowers and dust gathering.
Weaving
The yarn is more serious when the yarn is pure polyester or polyester yarn.
Suitable antistatic agents can be added in sizing to reduce static electricity during weaving, improve weaving efficiency and improve fabric quality.
Antistatic agent can form continuous conductive mould on the surface of the fiber, increase the conductivity of the fiber material, reduce the surface resistivity, and make the generated static electricity leak quickly, so as to achieve the effect of eliminating static electricity.
In addition, if
Slurry foam
Too much, the sizing rate is not easy to master, you can use defoamer.
It is recommended to use solid silicone as the first defoamer when partial alcoholysis of PVA slurry is used. If the amount of starch in the slurry is large and the protein content is high, the three butyl phosphate can be recommended.
Different defoamer should be selected for different types of foam. When necessary, mixing can be considered to achieve the ultimate goal of less dosage and better effect.
- Related reading
Several Problems In The Application Of Reactive Dye Digital Direct Jet Printing
|- News Republic | The US Estimates That The Price Of Cotton Will Continue To Rise This Year.
- Fashion brand | Spanish Dress Brand Aesop Easterly New Dress Debut
- Macro economy | World Economy: Left &Nbsp Or Right?
- News and information | Smiling Curves, Laughing And Fighting: Children's Clothing Industry: Stride Towards The Trillions Club
- neust fashion | Slim And Beautiful &Nbsp; Valentine'S Day Is The Ultimate Beauty.
- Stock school | High Margin Of Retail Safety: 2011: Textile Stocks Are Still Vulnerable.
- Gem | "The Incubated" Gem Is The First To List.
- Footwear industry dynamics | Chengdu Shoe Enterprises Actively Explore Bottlenecks To Break Through The Domestic Market
- Gem | Gem Rose 3.77% In The First Week After The Holiday
- News Republic | New Year'S Spring &Nbsp; Shaoxing Textile Enterprises Orders Still Panic At Hand.
- Ink Problems And Pre And Post Processing In Inkjet Digital Printing
- Several Problems In The Application Of Reactive Dye Digital Direct Jet Printing
- Breakthroughs In Key Common Technologies Of China'S Textile Industry
- 碳纖維產業從無到有實現“三初”
- 國產碳纖維行業發展呈現三大特點
- China'S First Provincial Cowboy Research Platform Settled In Wuhan Textile University
- Vojssen'S Printing And Dyeing Wastewater Treatment Technology Is Leading In China.
- The "Canopy Woven Composite" Standard Is Approved By The Federation.
- XTEP Builds "CNC Generation" Project To Facilitate Automatic Production
- Xinjiang Worries About The Cost And Can Not Receive Any Urgent Subsidies.